Bis zu 50 % günstiger als neu
3 Jahre rebuy Garantie
Professionelles Refurbishment
ElektronikMedien
Tipps & News
AppleAlle anzeigen
TabletsAlle anzeigen
HandyAlle anzeigen
Fairphone
AppleAlle anzeigen
iPhone Air Generation
GoogleAlle anzeigen
Pixel Fold
HonorAlle anzeigen
HuaweiAlle anzeigen
Honor Serie
NothingAlle anzeigen
OnePlusAlle anzeigen
OnePlus 11 GenerationOnePlus 12 Generation
SamsungAlle anzeigen
Galaxy XcoverWeitere Modelle
SonyAlle anzeigen
Weitere Modelle
XiaomiAlle anzeigen
Weitere Modelle
Tablets & eBook ReaderAlle anzeigen
Google
AppleAlle anzeigen
HuaweiAlle anzeigen
MatePad Pro Serie
MicrosoftAlle anzeigen
XiaomiAlle anzeigen
Kameras & ZubehörAlle anzeigen
ObjektiveAlle anzeigen
Samyang
System & SpiegelreflexAlle anzeigen
CanonAlle anzeigen
FujifilmAlle anzeigen
OlympusAlle anzeigen
PanasonicAlle anzeigen
SonyAlle anzeigen
WearablesAlle anzeigen
Fitness TrackerAlle anzeigen
SmartwatchesAlle anzeigen
Xiaomi
Konsolen & ZubehörAlle anzeigen
Lenovo Legion GoMSI Claw
NintendoAlle anzeigen
Nintendo Switch Lite
PlayStationAlle anzeigen
XboxAlle anzeigen
Audio & HiFiAlle anzeigen
KopfhörerAlle anzeigen
FairphoneGoogle
LautsprecherAlle anzeigen
GoogleYamahatonies
iPodAlle anzeigen

Handgeprüfte Gebrauchtware

Bis zu 50 % günstiger als neu

Der Umwelt zuliebe

Differential Scanning Calorimetry

G.W.H. Höhne (Gebundene Ausgabe, Englisch)

Keine Bewertungen vorhanden
Optischer Zustand
Beschreibung
Differential Scanning Calorimetry (DSC) is a well established measuring method which is used on a large scale in different areas of research, development, and quality inspection and testing. Over a large temperature range, thermal effects can be quickly identified and the relevant temperature and the characteristic caloric values determined using substance quantities in the mg range. Measurement values obtained by DSC allow heat capacity, heat of transition, kinetic data, purity and glass transition to be determined. DSC curves serve to identify substances, to set up phase diagrams and to determine degrees of crystallinity. This book provides, for the first time, an overall description of the most impor tant applications of Differential Scanning Calorimetry. Prerequisites for reliable measurement results, optimum evaluation of the measurement curves and esti mation of the uncertainties of measurement are, however, the knowledge of the theoretical bases of DSC, a precise calibration of the calorimeter and the correct analysis of the measurement curve. The largest part of this book deals with these basic aspects: The theory of DSC is discussed for both heat flux and power compensated instruments; temperature calibration and caloric calibration are described on the basis of thermodynamic principles. Desmearing of the measurement curve in different ways is presented as a method for evaluating the curves of fast transitions.
Dieses Produkt haben wir gerade leider nicht auf Lager.
ab 28,99 €
Derzeit nicht verfügbar
Derzeit nicht verfügbar

Handgeprüfte Gebrauchtware

Bis zu 50 % günstiger als neu

Der Umwelt zuliebe

Technische Daten


Erscheinungsdatum
14.05.1996
Sprache
Englisch
EAN
9783540590125
Herausgeber
Springer Berlin
Sonderedition
Nein
Autor
G.W.H. Höhne
Seitenanzahl
223
Einbandart
Gebundene Ausgabe
Buch Untertitel
An Introduction for Practitioners
Schlagwörter
Caliometry, information, Analyse, calorimeter, calorimetry, Thermal Analysis, Kalorimetrie, Dynamische Differenzkalorimetrie, Thermische Analyse
Thema-Inhalt
PNF - Analytische Chemie PNR - Physikalische Chemie
Höhe
235 mm
Breite
15.5 cm
-.-
Leider noch keine Bewertungen
Leider noch keine Bewertungen
Schreib die erste Bewertung für dieses Produkt!
Wenn du eine Bewertung für dieses Produkt schreibst, hilfst du allen Kund:innen, die noch überlegen, ob sie das Produkt kaufen wollen. Vielen Dank, dass du mitmachst!